Zn: Balance
|
JIS |
UNS |
EN |
Cu% |
Ni% |
Zn% |
|
C7701 |
C77000 |
CuNi18Zn27 |
53.5-56.5 |
16.5-19.5 |
Rem |
Mechanical Properties
|
Mechanical Properties for C77000 alloy |
||||
|
Alloy No |
Quality |
Tensile |
Elongation % |
Hardness Test HV |
|
Grade |
Strength |
|
|
|
|
|
(Kgf/mm |
|
|
|
|
C77000 |
1/2H |
55~66 |
≥8 |
150~210 |
|
H |
64~75 |
≥5 |
180~240 |
|
|
EH |
72~82 |
~ |
240~260 |
|
|
SH |
78~88 |
~ |
230~270 |
|
Application
C77000 /CuNi18Zn27 - mainly used in Liquid crystal oscillator component housing, medical machinery, slides for potentiometers, precision instruments, architecture, wind instruments, etc.